Iron Additive
+
  • Iron Additive

Product Details

Product Application

This product is suitable for increasing the iron (Fe) element content when configuring aluminum products, as a substitute for aluminum-iron intermediate alloys, with the following advantages:

1. High actual yield of the product, greater than 95%.

2. Rapid dissolution at low temperature, completely melted within 20 minutes above 720°C.

3. Easy storage and simple operation.

Usage Method

1. After the aluminum melts completely, stir the aluminum liquid up and down to make the temperature uniform.

2. Measure the temperature of the aluminum liquid, which should be at least above 720°C.

3. After reaching the temperature, remove the surface slag and add the required amount of additive.

4. After standing for 10 minutes, stir evenly for 5 minutes, then take a sample for testing.

5. After refining and slag removal, casting can be performed.

Iron Element Additive

Composition Analysis

Metal powder + balance

Metal powder

Iron: 75%—80%—85%—90%—95%

Balance

1. Sodium-free fluxing agent; 2. Aluminum powder; 3. Sodium-free fluxing agent + aluminum powder;

Color Mark

Red

Weight

20kg/box

Packaging

Plastic liner moisture-proof, cardboard box outer packaging

Remarks

Can also be produced according to requirements

Storage

This product should be stored in a dry and ventilated place to prevent moisture.

Shelf Life

Stored in a dry environment for 8 months

Iron Additive


This product is suitable for increasing the iron (Fe) content when configuring aluminum products, as a substitute for aluminum-iron intermediate alloys.
Iron Additive
+
  • Iron Additive

Keywords:

Iron Additive



Get Consultation Information for Free


Note: Please leave your contact information, our professionals will contact you as soon as possible!

Submit Now

Recommended Products


Focused on the research, production, sales, and service of aluminum non-ferrous metal fluxes, additives, and online degassing filtration equipment